Resin and adhesives

Mirrors built up until the late 1990s were constructed using polyester resin and Aerolite 306 glue. In my experience Aerolite 306 appears to break down after about 25 years, so glued joints failing is a common sight on older boats.
 
Since then most builders switched to epoxy resin for taping and epoxy resin plus thickening additives to make wood glue or to make fillets.  Today, the UK MCA recommends the use of epoxy systems.
 
In the UK the most commonly available brands are
Epoxy resin is superior to polyester in every respect apart from resistance to ultraviolet (UV) light degredation. Once a joint is complete, epoxy resin needs protecting by a good quality paint or varnish with a UV inhibitor.
 
 
 

Latest forum posts

More Topics »

Forthcoming Events

22 Jun 2019
Dalgety Bay Sailing Club
Scottish Championship & Northern Travellers
22 Jun 2019
Dalgety Bay Sailing Club
Scottish Championship & Northern Travellers
29 Jun 2019
Filey Sailing Club
Filey Regatta
29 Jun 2019
Filey Sailing Club
Filey Regatta
13 Jul 2019
Bassenthwaite Sailing Club
National Inland, Youth & Junior and Singlehanded Championships
13 Jul 2019
Bassenthwaite Sailing Club
National Inland, Youth & Junior and Singlehanded Championships
03 Aug 2019
Bassenthwaite Sailing Club
Bassweek Annual Regatta
03 Aug 2019
Bassenthwaite Sailing Club
Bassweek Annual Regatta
03 Aug 2019
Bassenthwaite Sailing Club
Bassweek Annual Regatta
03 Aug 2019
Bassenthwaite Sailing Club
Bassweek Annual Regatta