Resin and adhesives

Mirrors built up until the late 1990s were constructed using polyester resin and Aerolite 306 glue. In my experience Aerolite 306 appears to break down after about 25 years, so glued joints failing is a common sight on older boats.
 
Since then most builders switched to epoxy resin for taping and epoxy resin plus thickening additives to make wood glue or to make fillets.  Today, the UK MCA recommends the use of epoxy systems.
 
In the UK the most commonly available brands are
Epoxy resin is superior to polyester in every respect apart from resistance to ultraviolet (UV) light degredation. Once a joint is complete, epoxy resin needs protecting by a good quality paint or varnish with a UV inhibitor.
 
 
 

Latest forum posts

  • No posts to display.

Forthcoming Events

02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
02 Aug 2020
Brightlingsea Sailing Club
Pyefleet Week
09 Aug 2020
Clubs in the Falmouth area such as Restronguet SC
Falmouth Week
09 Aug 2020
Salcombe Yacht Club
Salcombe Gin – 2020 Salcombe Yacht Club Regatta
09 Aug 2020
Clubs in the Falmouth area such as Restronguet SC
Falmouth Week
09 Aug 2020
Salcombe Yacht Club
Salcombe Gin – 2020 Salcombe Yacht Club Regatta